Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.205 GPa | 29.7 ksi | MD |
Kuraray HYBRAR® BF2 Three Layer Blown Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |