Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 286 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.97 GPa
286 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
Tensile Modulus 1.97 GPa
286 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Tensile Modulus 1.97 GPa
286 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Tensile Modulus 1.97 GPa
286 ksi
1mm/min
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Tensile Modulus 1.97 GPa
286 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications.
Tensile Modulus 1.97 GPa
286 ksi
ASTM Data
Americas Styrenics Styron® 6010 High Impact Polystyrene  (discontinued **)
STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac..
Tensile Modulus 1.97 GPa
286 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Tensile Modulus 1.97 GPa
286 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi..
Tensile Modulus 1.97 GPa
286 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific ..
Tensile Modulus 1.97 GPa
286 ksi
ASTM Test
BASF Ultraform N 2640 Z2 UNC Q600 POM
Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength.
Tensile Modulus 1.97 GPa
286 ksi
ASTM D-638
Axiall 3020 Rigid PVC, Extrusion
Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G..
Tensile Modulus 1.97 GPa
286 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Tensile Modulus 1.97 GPa
286 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics GELOY CR7500 ASA
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
Copyright © lookpolymers.com All Rights Reserved