Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D 638 |
Shakespeare Isocorâ„¢ CF140ZI Nylon 6/66 Isocorâ„¢ CF140ZI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balan.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Spartech Centrex SP-6710 Weatherable Sheet Description: Weatherable SheetCentrex is a registered trademark of Bayer Corporation.Information provided by Spartech. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Spartech GELOY SP-6730 Weatherable Sheet Description: Weatherable SheetGeloy is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Spartech Weather-Pro Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Test |
Styrolution Terblend® N NM-19 ABS/PA6 (Dry) Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnumâ„¢ PG914 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D882 |
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compli.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
American Polymers API 425 Polystyrene API 425 is a medium impact grade of polystyrene for injection molding. API 425 has good gloss, easy flow and fast cycling properties.Applications: API 425 is widely used in cosmetic packaging, food.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics PREVEX W20 PPE+PS Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |