Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.38 GPa | 2666 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AE is a compound based on PA 66 rsin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Tensile Modulus | 18.38 GPa | 2666 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific) LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 18.38 GPa | 2666 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX07013 PA 66 (Europe-Africa-Middle East) LNP VERTON * RX07013 is a compound based on Nylon 66 resin containig Long Glass. Added features of this material include: Easy Molding and UV Resistant. |
|||
Tensile Modulus | 18.38 GPa | 2666 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Tensile Modulus | 18.38 GPa | 2666 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural. |
|||
Tensile Modulus | 18.38 GPa | 2666 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |