Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 25.5 GPa @Temperature 23.9 °C |
3700 ksi @Temperature 75.0 °F |
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D3039 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Tensile Modulus | 25.5 GPa @Temperature 23.9 °C |
3700 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati.. |
|||
Tensile Modulus | 25.5 GPa @Temperature 23.9 °C |
3700 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Tensile Modulus | 25.5 GPa | 3700 ksi | ASTM D638 |
Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Compression Grade Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimens.. |
|||
Tensile Modulus | 25.5 GPa | 3700 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
Tensile Modulus | 25.5 GPa | 3700 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 25.5 GPa | 3700 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65 Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I.. |
|||
Tensile Modulus | 25.5 GPa | 3700 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65 Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I.. |