Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.72 GPa | 249 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 2.0 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 2 in/min; ASTM Test |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | ASTM Test |
Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 2.0 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EC6600 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Lithographic sheetPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Excellent printabilityMatte surface finishHigh hea.. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMT222 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by good stiffness/toughness balance and designed for automotive interior applications in which good surface finish and g.. |
|||
Tensile Modulus | 1.71 GPa | 249 ksi | Storage |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | 1 mm/min |
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |
|||
Tensile Modulus | 1.72 GPa | 249 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ PP-CP1/000 HF6 Black Polypropylene Impact Copolymer (PP Impact Copolymer) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |