Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.62 GPa | 235 ksi | 2.0 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 1mm/min |
Eastman Tenite 105-33 Cellulose Acetate
(discontinued **) 33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific) LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | ASTM D638 |
Elastomer Engineering Elastamide XP91 Elastomer Modified RIM Nylon 6 Information supplied by Elastomer Engineering. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 2.0 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Modulus | 1.62 GPa | 235 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |