Polymer Property : Tensile Modulus = 228 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.57 GPa
228 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® FXE173R PC
This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 1.57 GPa
228 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® SFX173RU PC
SFX173RU is a transparent SecurFX grade with high flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.
Tensile Modulus 1.57 GPa
228 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® SFX173RU PC (Asia Pacific)
SFX173RU is a transparent SecurFX grade with high flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.
Tensile Modulus 1.57 GPa
228 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MX01767C PP
LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Tensile Modulus 1.57 GPa
228 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON MX10301C PP
LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Tensile Modulus 1.57 GPa
228 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Modulus 1.57 GPa
228 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Modulus 1.57 GPa
228 ksi
Film M.D.; ASTM D882
Eastman Eastman Embrace Copolyester for Extrusion/Cast Film
Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood ..
Tensile Modulus 1.57 GPa
228 ksi
Storage
Epoxy Technology EPO-TEK® B912-8 Epoxy
Product Description: A single component, thermally and electrically conductive, epoxy adhesive designed for semiconductor die attach and circuit assembly applications. Its unique features are a pot..
Tensile Modulus 1.57 GPa
228 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..