Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 22.8 GPa | 3310 ksi | |
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Tensile Modulus | 22.8 GPa | 3310 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to.. |
|||
Tensile Modulus | 22.8 GPa | 3310 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Tensile Modulus | 22.8 GPa | 3300 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® SF-30CF/000 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 22.8 GPa | 3300 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Modulus | 22.8 GPa | 3310 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Tensile Modulus | 22.8 GPa | 3300 ksi | 50 mm/min; ASTM D638 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |