Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 21.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 21.5 GPa
3120 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA)  (Unverified Data**)
Ixef 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss. - B..
Tensile Modulus 21.5 GPa
3120 ksi
ISO 527-2
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral
Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss...
Tensile Modulus 21.5 GPa
3120 ksi
ASTM-D790
Polyram Polytron A60B02 Nylon 66, Chemically Coupled 60% Long Fiber
A CHEMICALLY COUPLED 60% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Tensile Modulus 21.5 GPa
3120 ksi
ASTM-D790
Polyram Polytron A60N02 Nylon 66, Chemically Coupled 60% Long Fiber
A CHEMICALLY COUPLED 60% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Tensile Modulus 21.5 GPa
3120 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® 1SVX-65H black 9288 PA1010-GF65
Product Description: Grilamid 1SVX-65H black is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources Exc..
Tensile Modulus 21.5 GPa
3120 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65
Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E..
Tensile Modulus 21.5 GPa
3120 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30
Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca..
Tensile Modulus 21.5 GPa
3120 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60
Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory..
Tensile Modulus 21.5 GPa
3120 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60
Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac..
Tensile Modulus 21.5 GPa
3120 ksi
transverse; ISO 527-4/5
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..
Tensile Modulus 21.5 GPa
3120 ksi
ASTM D638
LNP Lubricomp® OCL-4036 Polyphenylene Sulfide, Carbon Fiber Reinforcement, PTFE Lubricant  (discontinued **)&l
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..