Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.24 GPa | 2065 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |