Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.2 GPa | 2930 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PC-30CF/000 BLACK Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Modulus | 20.2 GPa | 2930 ksi | ASTM D638 |
Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Tensile Modulus | 20.2 GPa | 2930 ksi | ISO 527 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |