Mechanical Properties Metric English Comments
Tensile Modulus 2.53 GPa
367 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2710 Amber 9360 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.53 GPa
367 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2710 Amber 9375 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.53 GPa
367 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging 2710 Polyvinyl Chloride, Rigid (PVC, Rigid)
This product is available in opaque and transparent colors.Information provided by PolyOne
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycolac® HMG47MD ABS
General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Tensile Modulus 2.53 GPa
367 ksi
ASTM D638
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products.
Tensile Modulus 2.53 GPa
367 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ SF M7100 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.53 GPa
367 ksi
Type I, 51 mm/min; ASTM D638
PolyOne Geon™ SF M7120 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS
LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare.
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer
INNOPOL® CS 2-3120 BPLU 9H0017 is a 20% talc filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3120 BPLU 9H0017 is developed for producing injection molded au..
Tensile Modulus 2.53 GPa
367 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer
LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant.
Tensile Modulus 2.53 GPa
367 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® HX3091HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only.
Tensile Modulus 2.53 GPa
367 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus.
Tensile Modulus 2.53 GPa

@Temperature -100 °C
367 ksi

@Temperature -148 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur..
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min
Arkema Group Nakan® RPX 301 L PVC, Rigid Extrusion Grade
NAKAN RPX 301 L is a rigid polyvinyl chloride compound developed for extrusion of transparent profiles for outdoor applications.ISO data provided by the manufacturer, Arkema.
Tensile Modulus 2.53 GPa
367 ksi
same value from ASTM and ISO test.
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)  (discontinued **)
Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions..
Tensile Modulus 2.53 GPa
367 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL FP5140HF PPE+PS
Noryl*FP5140HF is an unfilled, injection moldable modified polyphenylene ether resin with an ISO306 Vicat B/120 of 100 deg C. Designed for good dimensional stability and high flow, this resin also u..
Tensile Modulus 2.53 GPa

@Temperature -100 °C
368 ksi

@Temperature -148 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)