Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.33 GPa | 338 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD171R PC Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD171R PC (Asia Pacific) Transparent/transluscent PC for light diffusion special effects. MFR of 25.0. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Colorcomp DX98735 PC LNP COLORCOMP* DX98735 is a compound based on Polycarbonate resin containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP DX98735H PC LNP* COLORCOMP* DX98735H is an unfilled Polycarbonate resin. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | ISO 527-2 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific) LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Tensile Modulus | 2.33 GPa @Thickness 3.20 mm |
338 ksi @Thickness 0.126 in |
5 mm/min, Injection Molded; ASTM D638 |
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm.. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | ISO 527-2 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | ISO 527-2 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | ISO 527-2 |
Styron Pulse® 2000EZ PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
Tensile Modulus | 2.33 GPa @Thickness 4.00 mm |
338 ksi @Thickness 0.157 in |
Injection Molded; ISO 527-2 |
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi.. |
|||
Tensile Modulus | 2.33 GPa @Temperature -20.0 °C |
339 ksi @Temperature -4.00 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Modulus | 2.33 GPa | 338 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |