Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.31 GPa | 335 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 104R PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® IR2840 PC 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7691 PC UV stabilized clear polycarbonate formula for internal uses only. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | ASTM D638 |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | |
Ineos ABS Lustran® 448 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 50 mm/min; ISO 527-2/50; ASTM D638 |
Styron CALIBREâ„¢ 302V-6 LD Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 LD HC18010009 Polycarbonate is an opalescent white extrusion-grade resin containing a proprietary light diffusion package that offers an excellent combination of light.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | ASTM D638 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 2.31 GPa | 335 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® SD1318 PC High viscosity, UV stabilized multi purpose grade. |