Mechanical Properties Metric English Comments
Tensile Modulus 2.29 GPa
332 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® ADX1016R PC (Europe-Africa-Middle East)
Lexan Copolymer resin with improved chemical resistance, available only in limited colors.
Tensile Modulus 2.29 GPa
332 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp DP0039 PC
LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.29 GPa
332 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
Tensile Modulus 2.29 GPa
332 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
Tensile Modulus 2.29 GPa
332 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon
LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant.
Tensile Modulus 2.29 GPa
332 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus.
Tensile Modulus 2.29 GPa
332 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL PX0844 PPE+PS
PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability.