Mechanical Properties Metric English Comments
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® 4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® HPH4504 PPC
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific)
Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only.
Tensile Modulus 2.09 GPa
303 ksi
1mm/min
Eastman Eastar DN102 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Lexan® ML5472 PC
Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.09 GPa

@Thickness 3.20 mm
303 ksi

@Thickness 0.126 in
1mm/min; ASTM D638
LG Chemical ALPHALAC SG910 HIPS
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA..
Tensile Modulus 2.09 GPa
303 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific)
LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP NXCY620 PC+ABS
LNP* LUBRICOMP* NXCY620 is a compound based on Cycoloy* XCY620 containing Silicone. Added feature of this material is: Lubricant.
Tensile Modulus 2.09 GPa
303 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP
SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met..
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA 11 (Asia Pacific)
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing Glass Bead.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® V3900WX PBT+PC
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
Tensile Modulus 2.09 GPa
303 ksi
1mm/min
Eastman Eastar 6763 PETG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Tensile Modulus 2.09 GPa

@Temperature 120 °C
303 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned)
Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic..
Tensile Modulus 2.09 GPa
303 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® HPH4504H PPC
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Tensile Modulus 2.09 GPa
303 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC
LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated.