Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.03 GPa | 294 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 1mm/min |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 2.03 GPa | 295 ksi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Tensile Modulus | 2.03 GPa | 295 ksi | ASTM D638 |
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Tensile Modulus | 2.03 GPa | 295 ksi | ASTM-D638 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Tensile Modulus | 2.03 GPa | 295 ksi | ASTM-D638 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Europe-Africa-Middle East) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | ASTM D638 |
Eastman Drystar 0325 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | ASTM D638 |
Eastman Drystar 0603 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s.. |
|||
Tensile Modulus | 2.03 GPa @Temperature -20.0 °C |
294 ksi @Temperature -4.00 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Modulus | 2.03 GPa | 294 ksi | 1 mm/min |
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good.. |