Polymer Property : Tensile Modulus = 19.78 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 19.78 GPa
2869 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Tensile Modulus 19.78 GPa
2869 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 19.78 GPa
2869 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.