Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 186 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.28 GPa
186 ksi
Storage
Epoxy Technology EPO-TEK® B9021-6 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
Tensile Modulus 1.28 GPa
186 ksi
1 mm/min
Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned)
Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier ..
Tensile Modulus 1.28 GPa
186 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 527
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11
Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic..
Copyright © lookpolymers.com All Rights Reserved