Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.14 GPa | 2631 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Tensile Modulus | 18.14 GPa | 2631 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS (Asia Pacific) LNP* Lubricomp* OCP36 is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, Lubricants, Bearing Grade. Added features of this material include: Internally Lubricated, Electric.. |
|||
Tensile Modulus | 18.14 GPa | 2631 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Bearing Grade, Electrically Conductive, Wear R.. |
|||
Tensile Modulus | 18.14 GPa | 2631 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing Bearing Grade, Carbon Fiber, Lubricants. Added features of this material include: Electrically Conductive. |