Mechanical Properties Metric English Comments
Tensile Modulus 12.2 GPa
1770 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
Tensile Modulus 12.2 GPa
1770 ksi
ASTM D638
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Tensile Modulus 12.2 GPa
1770 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced
PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS.
Tensile Modulus 12.2 GPa
1770 ksi
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor..
Tensile Modulus 12.2 GPa
1770 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific)
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Tensile Modulus 12.2 GPa
1770 ksi
ASTM D638
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Tensile Modulus 12.2 GPa
1770 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East)
LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific)
LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66
LNP* THERMOCOMP* RF008H is a compound based on Nylon 66 containing 40% Glass Fiber. Added feature of this grade is: Healthcare.
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66
LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber.
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RX10405H PA 66
LNP* Thermocomp* RX10405H is a compound based on Nylon 6/6 containing Carbon Fiber. Characteristics of this grade are: Healthcare.
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527-1
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber
SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DE003E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE003E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Tensile Modulus 12.2 GPa
1770 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
Tensile Modulus 12.2 GPa
1770 ksi
ISO 527-1/-2
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Information provided by Unitika Ltd.
Tensile Modulus 12.2 GPa
1770 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50
Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010..
Tensile Modulus 12.2 GPa
1770 ksi
Conditioned; ASTM D638
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon PX98038 PA 6 (Europe-Africa-Middle East)
LNP* STATKON* PX98038 is a compound based on PA6 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include : Flame Retardant, Electrically Conductive, Heat Stabilized.This ..
Tensile Modulus 12.2 GPa
1770 ksi
ASTM D638
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Tensile Modulus 12.2 GPa
1770 ksi
cond; ISO 527-1/-2
DSM Novamid® MC112LG55 C10 PA6-GF55
55% Glass Reinforced
Tensile Modulus 12.2 GPa
1770 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..