Mechanical Properties Metric English Comments
Tensile Modulus 11.8 GPa
1710 ksi
STN EN ISO 527-2
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance
PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved..
Tensile Modulus 11.79 GPa
1710 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6
LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant
Tensile Modulus 11.79 GPa
1710 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
Tensile Modulus 11.8 GPa
1710 ksi
ISO 527-1/-2
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance
Tensile Modulus 11.8 GPa
1710 ksi
ISO 527 Type 1A
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
Tensile Modulus 11.8 GPa
1710 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ420 PBT
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Tensile Modulus 11.8 GPa
1710 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Tensile Modulus 11.8 GPa
1710 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Tensile Modulus 11.8 GPa
1710 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Tensile Modulus 11.8 GPa
1710 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ420HP PBT
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Tensile Modulus 11.8 GPa
1710 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Tensile Modulus 11.8 GPa
1710 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RX10409D PA 66
LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural.
Tensile Modulus 11.8 GPa
1710 ksi
ASTM D638
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Tensile Modulus 11.8 GPa
1710 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel..
Tensile Modulus 11.8 GPa
1710 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN LT51G35HSLR BL661A Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Laser Weldable PPA High Performance Polyamide Information provided by DuPont Performance Polymers
Tensile Modulus 11.8 GPa
1710 ksi
ISO 527-1
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced
PEEK-GF30Information provided by BARLOG plastics GmbH.
Tensile Modulus 11.8 GPa

@Temperature 23.0 °C
1710 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..
Tensile Modulus 11.8 GPa
1710 ksi
ASTM D638
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Tensile Modulus 11.8 GPa
1710 ksi
ISO 527-1/2
Radici Radiflam® BRV300 AE Polybutylene Terephthalate
PBT Self-extinguishing glass-fiber reinforced with halogenInformation provided by Radici group.
Tensile Modulus 11.8 GPa
1710 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East)
LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact.