Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.38 GPa | 2521 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EC004XXQ PEI LNP* THERMOCOMP* EC004XXQ is a compound based on Polyetherimide containing 20% Carbon Fiber. |