Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.16 GPa | 1619 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific) LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 11.16 GPa | 1619 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON JX89626 PES LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 11.16 GPa | 1619 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
Tensile Modulus | 11.16 GPa | 1619 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Tensile Modulus | 11.16 GPa | 1619 ksi | ISO 527 |
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram. |