Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.79 GPa | 1565 ksi | ASTM D638 |
Plenco 51130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform.. |
|||
Tensile Modulus | 10.79 GPa @Temperature -40.0 °C |
1565 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |