Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.14 GPa | 2196 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |