Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.2 GPa | 1480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Tensile Modulus | 10.2 GPa @Temperature 23.0 °C |
1480 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Tensile Modulus | 10.2 GPa @Temperature 23.0 °C |
1480 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527 |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | Transverse; ASTM D3039 |
Greene Tweed WR™ 525 PEEK, Carbon Filled WR®525 is a thermoplastic composite consisting of carbon fiber in a PEEK matrix. Because of its unique thermal expansion properties, WR525 is deal for use as impeller wear rings, bushings and ca.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 135 DUS008 000000 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific) LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ASTM D638 |
Plenco 3356 Phenolic, Granular, Transfer Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527-1/-2 |
DSM Akulon® K224-LG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1017GH33 BK701 PA6-GF33 33% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR BK851 is a 30% glass fiber reinforced flame retardant black polybutylene tere.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 935 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 BK505 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1mm/min; ISO 527 |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1mm/min; ISO 527 |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527 |
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 572 |
Bulk Molding Compounds BMC 665 Mineral filled, 20% glass reinforced polyester molding compound Description: BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527 |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated. |
|||
Tensile Modulus | 10.2 GPa | 1480 ksi | |
LATI Laticonther 75 GR/50 PBT, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Tensile Modulus | 10.2 GPa @Temperature 23.0 °C |
1480 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |