Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.80 GPa | 1420 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Tensile Modulus | 9.81 GPa | 1420 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Modulus | 9.79 GPa | 1420 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON MV007SU PP (Europe-Africa-Middle East) LNP* VERTON * MV007SU is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilizedl. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.79 GPa | 1420 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ASTM D638 |
Plenco 4349 Phenolic, Granular, Compression Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ASTM-D790 |
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527 |
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber 30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 9.77 GPa @Temperature -50.0 °C |
1420 ksi @Temperature -58.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Tensile Modulus | 9.79 GPa | 1420 ksi | ASTM D638 |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Tensile Modulus | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 30 W1 000000 Nylon 6, 30% Glass Fiber PA 6, Injection molding grade, 30% glass fibers, weather stabilized |