Polymer Property : Tensile Modulus = 14.79 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 14.79 GPa
2145 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA
LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.