Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.69 GPa | 2131 ksi | ASTM D638 |
Plenco 50045 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Tensile Modulus | 14.69 GPa | 2131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Tensile Modulus | 14.69 GPa | 2131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Tensile Modulus | 14.69 GPa | 2131 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |