Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.800 - 0.900 GPa | 116 - 131 ksi | |
Addcomp PRIEX® Ionomer 48101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Tensile Modulus | 0.800 - 0.900 GPa | 116 - 131 ksi | |
Addcomp PRIEX® Ionomer 45101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |