Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.793 GPa | 2000.5 ksi | ASTM D-638 |
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by.. |