Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.40 GPa | 1220 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Opnyl OP6GF43 Nylon 6, 43% Glass Reinforced, Dry Nylon 6 - Glass reinforced (43 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527-1/2 |
Radici Radilon® SERV3808 K (dry) Nylon 6 Heat stabilized glass-fiber reinforced with high impact strengthInformation provided by Radici group. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 |
Radici Radilon® WIT 30/28 Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by WIT technology.Information provided by Radici group. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features include; Internally Lubricated, Easy Molding. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 |
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 8.41 GPa | 1220 ksi | 20% Glass RTM Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527-1/-2 |
Lanxess Pocan® KL 1-7033 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, impact modified |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | |
LATI Latiohm 90/13-09 PD01 G/10 PPOm, 10% Glass Fiber Reinforced Semiconductive/dissipative product based on Modified Polyphenylene Oxide (PPOm). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Tensile Modulus | 8.41 GPa | 1220 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, Conditioned Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East) LNP*Lubricomp* QFL36 is a compound based on PA 6/10 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Tensile Modulus | 8.42 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 8.41 GPa | 1220 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10 LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 8.43 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RX08401 PA 66 LNP* Thermocomp* RX08401 is a compound based on Nylon 66 containing Glass Fiber. Added feature of this grade include: Impact Modified. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KEL22A Acetal Homopolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL22A is a compound based on Acetal Homopolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | dry; ISO 527 |
Ter Hell Plastic Terez® PBT 7100 GF 30 Polybutylene Terephthalate, 30% Glass Fiber Description: PBT, 30% glass fiber reinforced.Application: Suitable for injection molding applications.Information provided by Ter Hell Plastic GMBH. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ASTM D638 |
Plenco 2408 Phenolic, Granular, Injection Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | ASTM D638 |
Plenco 4301 Phenolic, Granular, Injection Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR BK099 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR BK099 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Tensile Modulus | 8.38 GPa @Temperature -20.0 °C |
1220 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Tensile Modulus | 8.40 GPa | 1220 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON KEL32 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL32 is a compound based on Acetal Copolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |