Polymer Property : Tensile Modulus = 1200 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.30 - 8.30 GPa
479 - 1200 ksi
MD; ISO 527 / PA_098
Quadrant Plastic Composites GMT Glass-Mat-Reinforced Thermoplastic
This semi-finished product in panel form was developed primarily as a substitute for metals (steel, aluminum etc.) and its main purchasers can be found in the automotive industry. This is where it i..