Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.88 GPa | 1868 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 12.88 GPa | 1868 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE004ER PC LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release. |