Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.2 GPa | 1770 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | ASTM D638 |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | |
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific) LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East) LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific) LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008 |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF008H PA 66 LNP* THERMOCOMP* RF008H is a compound based on Nylon 66 containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RX10405H PA 66 LNP* Thermocomp* RX10405H is a compound based on Nylon 6/6 containing Carbon Fiber. Characteristics of this grade are: Healthcare. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DE003E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE003E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6 LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | ISO 527-1/-2 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon PX98038 PA 6 (Europe-Africa-Middle East) LNP* STATKON* PX98038 is a compound based on PA6 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include : Flame Retardant, Electrically Conductive, Heat Stabilized.This .. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | ASTM D638 |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | cond; ISO 527-1/-2 |
DSM Novamid® MC112LG55 C10 PA6-GF55 55% Glass Reinforced |
|||
Tensile Modulus | 12.2 GPa | 1770 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |