Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.76 GPa | 1706 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 11.76 GPa | 1706 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 11.76 GPa | 1706 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT LNP LUBRICOMP* WFP36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 11.76 GPa | 1706 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Asia Pacific) LNP LUBRICOMP* WFP36 is a compound based on Polybutylene Terephalate resin containing Silicone, Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 11.76 GPa | 1706 ksi | DAM; ISO 527 Type 1 A |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |