Polymer Property : Tensile Modulus = 10.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0740 GPa

@Temperature 23.0 °C
10.7 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a..
Tensile Modulus 0.0740 GPa
10.7 ksi
BASF Lucalen® A 3110 M Ethylene/Acrylate Copolymer
Economical composite films together with PE-LD; primers for aluminum/steel composites; coatings for paper board, aluminum and steel (e.g. for pipes used to transport petroleum, gas, etc.)Data was co..
Tensile Modulus 0.0740 GPa
10.7 ksi
BASF Lucalen® A 3110 M Q 244 Ethylene/Acrylate Copolymer
Data was collected by ISO methods and provided by BASF.
Tensile Modulus 0.0740 GPa
10.7 ksi
BASF Lucalen® A 3110 M Q 270 Ethylene/Acrylate Copolymer
Data was collected by ISO methods and provided by BASF.
Tensile Modulus 0.0740 GPa
10.7 ksi
BASF Lucalen® A 3120 M Ethylene/Acrylate Copolymer
Suitable in similar manner as Lucalen A 2920 M or also as a material for coating aluminum, steel, paper and cardboard. Also for processing pipes for transporting petroleum, gas, etc.Data was collec..