Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.33 GPa @Temperature 23.0 °C |
1498 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
Tensile Modulus | 10.33 GPa | 1498 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK645FR BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR BK851 is a flame retardant 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL.. |