Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.93 GPa | 280 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Ravago Manufacturing Americas Hysun™ 383 ASA
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics PREVEX W20 PPE+PS (Asia Pacific) Automotive. PPE alloy. High flow/impact. Instrument panels and interior trim components. HDT 210F. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D 638 |
Shakespeare Isocorâ„¢ CF140ZI Nylon 6/66 Isocorâ„¢ CF140ZI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balan.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D2000P PC LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D 638 |
Shakespeare Isocorâ„¢ CU145SI Nylon 6/66 Isocorâ„¢ CU145SI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balan.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Spartech SP-9050 Low Gloss ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Spartech Weather-Pro Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Test |
Styrolution Terblend® N NM-11 ABS/PA6 (Dry) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Test |
Styrolution Terblend® N NM-19 ABS/PA6 (Dry) Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Test |
Styrolution Terblend® N NMX04 ABS/PA6 (Dry) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM Data |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT 4.2 specific gravity, PBT, gray |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | |
Master Bond EP21LV35Med Two Component, Flexible USP Class VI Epoxy System Master Bond Polymer System EP21LV3/5Med is a two part, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting that cures flexible. It cures readil.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
Videolar 825 E High Impact Polystyrene (HIPS) Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: St.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D-638 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Tensile Modulus | 1.93 GPa | 280 ksi | ASTM D638 |
American Polymers API 425 Polystyrene API 425 is a medium impact grade of polystyrene for injection molding. API 425 has good gloss, easy flow and fast cycling properties.Applications: API 425 is widely used in cosmetic packaging, food.. |