Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.74 GPa | 252 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC X THC 1101 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Edgetek® XT X XT 1001 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | 1mm/min |
Eastman Tenite 383A-08 Cellulose Acetate Propionate
(discontinued **) 8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | 1mm/min |
Eastman Tenite 371A-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | after conditioning; ISO 527 |
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.Polypropylene PPC 3150 MX5 is .. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | XY direction; ASTM D638 |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Tensile Modulus | 1.74 GPa | 253 ksi | ASTM D638 |
Amco Amalloy® B9714 Polymer Alloy Amco Amalloy B9714 is a clear performance copolymer with exceptional clarity and toughness.High elongation before breakage, good melt Flow.Information provided by Amco Plastic Materials. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, Conditioned Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Tensile Modulus | 1.74 GPa | 252 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |