Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.73 GPa | 251 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 1.73 GPa | 251 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Tensile Modulus | 1.73 GPa | 251 ksi | 2in/min; ASTM D882 |
Styrolution Styrolux® GH 62 SBC Description: Styrolux® GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warp.. |
|||
Tensile Modulus | 1.73 GPa | 252 ksi | Storage |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Tensile Modulus | 1.73 GPa | 251 ksi | Storage |
Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy Material Description: A single component, low viscosity, UV curable adhesive designed for curing in seconds. It is an all-purpose, general adhesive for optical applications including fiber optic co.. |
|||
Tensile Modulus | 1.73 GPa | 251 ksi | 1 mm/min |
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Dry) Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite.. |
|||
Tensile Modulus | 1.73 GPa | 251 ksi | 2 in/min; ASTM Test |
BASF Styroclear GH 62 SBC Styroclear GH 62 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance.. |