Mechanical Properties Metric English Comments
Tensile Modulus 1.62 GPa
235 ksi
2.0 in/min; 0.050" thickness; ASTM D-638
Chevron Phillips EC6400 HIPS - High Impact Polystyrene  (discontinued **)
Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface ..
Tensile Modulus 1.62 GPa
235 ksi
1mm/min
Eastman Tenite 105-33 Cellulose Acetate  (discontinued **)
33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Tensile Modulus 1.62 GPa
235 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP
LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant.
Tensile Modulus 1.62 GPa
235 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 1.62 GPa
235 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific)
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 1.62 GPa
235 ksi
ASTM D638
Elastomer Engineering Elastamide XP91 Elastomer Modified RIM Nylon 6
Information supplied by Elastomer Engineering.
Tensile Modulus 1.62 GPa
235 ksi
2.0 in/min; 0.050" thickness; ASTM D-638
Chevron Phillips EB6400 HIPS - High Impact Polystyrene
Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface ..
Tensile Modulus 1.62 GPa
235 ksi
1 mm/min
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Tensile Modulus 1.62 GPa
235 ksi
1 mm/min
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..