Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | chs 2 in/min; ASTM D638 |
Network Polymers NPS 90-0802 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Tensile Modulus | 1.59 - 1.66 GPa | 231 - 241 ksi | ASTM D638 |
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | TM R050-36 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | ASTM Data |
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PE-30MC-20TC/000 High Density Polyethylene (HDPE), Talc Filled
(discontinued **) Description/Features:Mica FilledTalc FilledInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 1mm/min |
Eastman Tenite 371A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 1mm/min |
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | |
Saint-Gobain Rulon® 125 Bearing/Seal PTFE Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor.. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Tensile Modulus | 1.59 GPa | 231 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Tensile Modulus | 1.59 - 1.66 GPa | 231 - 241 ksi | ASTM D638 |
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |
|||
Tensile Modulus | 1.59 GPa | 230 ksi | ASTM D638 |
American Polymers API 550 Polystyrene API 550 is a high impact grade of polystyrene. It is characterized by good impact and processability.Applications: API 550 is widely used in housewares, toys, containers, appliance parts, speaker h.. |