Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.449 GPa @Temperature 150 °C |
210.2 ksi @Temperature 302 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |