Polymer Property : Tensile Modulus = 0.520 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.520 GPa
75.4 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12
Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng..
Tensile Modulus 0.520 GPa
75.4 ksi
1 mm/min
Arkema Group Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11-P,EHL,22-004Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.Flexibility. High impact strength. Very good chemical resistan..
Tensile Modulus 0.520 - 0.750 GPa
75.4 - 109 ksi
ISO 527
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Tensile Modulus 0.520 GPa
75.4 ksi
ISO 527-1/-2
DSM Arnitel® PM650 General Purpose Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Modulus 0.520 GPa
75.4 ksi
ISO 527-1/-2
DSM Arnitel® PM650 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..