Mechanical Properties Metric English Comments
Tensile Modulus 0.450 - 0.750 GPa
65.3 - 109 ksi
ASTM D638
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Tensile Modulus 0.450 - 0.550 GPa
65.3 - 79.8 ksi
ISO 527-2
Borealis BD212CF Polypropylene Copolymer
BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, l..
Tensile Modulus 0.450 - 0.550 GPa
65.3 - 79.8 ksi
ISO 527-2
Borealis BD712CF Polypropylene Copolymer
BD712CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD712CF is recommended for food packaging..
Tensile Modulus 0.450 GPa
65.3 ksi
ISO 527-2
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating
Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the..
Tensile Modulus 0.450 GPa
65.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610
Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati..
Tensile Modulus 0.450 GPa
65.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610
Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic..
Tensile Modulus 0.450 GPa
65.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I
Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is ..
Tensile Modulus 0.450 GPa
65.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I
Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610..
Tensile Modulus 0.450 GPa
65.3 ksi
Foaming Direction
Cymat A35620SC 020SS Stabilized Aluminum Foam
Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it ..
Tensile Modulus 0.450 GPa
65.3 ksi
1 mm/min; ISO 527
Eurostar Starpylen HU 70E3 HDPE, Injection Molding
Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar.
Tensile Modulus 0.450 GPa
65.3 ksi
1 mm/min; ISO 527
Eurostar Starpylen MH0200A HDPE, Injection Molding
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 0.450 GPa
65.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 20 X PA12-I
Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th..
Tensile Modulus 0.450 GPa
65.3 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 20 X PA12-I
Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th..
Tensile Modulus 0.450 GPa
65.3 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® L 25 W 40 PA12
Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid ..
Tensile Modulus 0.450 GPa
65.3 ksi
MD; ASTM D882-A
Borealis Borstar® FB4370 Medium Density Polyethylene
Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap..