Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.360 - 0.480 GPa @Thickness 2.00 mm |
52.2 - 69.6 ksi @Thickness 0.0787 in |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Tensile Modulus | 0.360 GPa | 52.2 ksi | ISO 527-1/-2 |
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P40 Nylon, conditioned Hiprolon® 11ESNNHL P40 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact.. |
|||
Tensile Modulus | 0.360 GPa | 52.2 ksi | cond; ISO 527-1/-2 |
DSM Novamid® ST145 NAT PA6-I Impact Modified, Injection Molding |
|||
Tensile Modulus | 0.360 GPa | 52.2 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 X PA12-I Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m.. |
|||
Tensile Modulus | 0.360 GPa | 52.2 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 22A W 40 X PA12-I Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st.. |
|||
Tensile Modulus | 0.360 GPa | 52.2 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube.. |
|||
Tensile Modulus | 0.360 GPa @Temperature 110 °C |
52.2 ksi @Temperature 230 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.360 GPa @Temperature 120 °C |
52.2 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Tensile Modulus | 0.360 GPa @Temperature 120 °C |
52.2 ksi @Temperature 248 °F |
ISO Data |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Tensile Modulus | 0.360 - 0.480 GPa @Thickness 2.00 mm, Temperature 23.0 °C |
52.2 - 69.6 ksi @Thickness 0.0787 in, Temperature 73.4 °F |
Type IV, 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |