Polymer Property : Tensile Modulus = 0.170 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Tensile Modulus 0.170 GPa
24.7 ksi
MD; ASTM D882-A
Borealis FG5190 Linear Low Density Polyethylene
FG5190 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes Antioxidant. The grade is developed for medium and heavy duty bags, bags and bin liners, dual stretch films, and film..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Eastman Eastman AP005 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Eastman Eastman AP006 Copolyester
Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Eastman Eastman AP007 Copolyester
Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Eastman Neostar FN005 Elastomer
Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Eastman Neostar FN006 Elastomer
Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and ..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D638
Eastman Neostar FN007 Elastomer
Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol..
Tensile Modulus 0.170 GPa
24.7 ksi
1 mm/min
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 38.1 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Tensile Modulus 0.170 GPa
24.7 ksi
ASTM D882
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..